Designation by Standards
Brand Name | Ravne No. | Mat. No. | DIN | EN | AISI |
20MC5 | 203 | 1.7147 | 20MnCr5 | - | - |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
0.19 | max. 0.10 | 1.15 | 1.25 | - | max. 0.30 | - | - | - |
Description
Alloyed carbon steel.
Applications
Higher stressed components – gears, cranks, crankschafts, switch
components, etc.
Physical properties (avarage values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 210
Density [g/cm3]: 7.85
Soft Annealing
Heat to 650-700oC, cool slowly. This will produce a maximum Brinell hardness of
217.
Carburizing
880-980 oC, water, oil, air, hot quenching 150-250oC or case hardening box.
Core hardening
Temperature: 860-900oC.
Surface hardening
Tempertaure: 720-820oC, oil, water or hot quenching.
Tempering
Tempering temperature: 150-200oC.
Forging
Hot forming temperature: 1150-850oC.
Machinability
No data.
Forms manufactured: Please see the Dimensional Sales Program.
Disclaimer
The information and data presented herein are typical or average
values and are not a guarantee of maximum or minimum values.
Applications specifically suggested for material described herein
are made solely for the purpose of illustration to enable the
reader to make his own evaluation and are not intended as
warranties, either express or implied, of fitness for these or
other puposes. There is no representation that the recipient of
this literature will receive updated editions as the become
available.
![]() |